POLIMIN PC-5 FIBRE REINFORCED SCREED cement screed for arranging and leveling floors, before laying tiles and other coatings, inside and outside buildings.
Technological properties of the PC-5 screed allow leveling the surface of existing concrete and cement-sand screeds with a graded strength of at least 20 MPa before laying facing tiles, other floor layers: self-leveling floors, etc. The screed allows for the arrangement of water-heated floor systems in strict compliance with the recommendations of the manufacturer of these systems, the thickness of the mortar layer above the heating element must be at least 25 mm.
Thanks to the improved formula, the product provides:
• easy distribution and leveling of the screed at an angle (performance of the screed)
• wide range of layer thicknesses (10–100* mm) ensures its use in various structures
• compressive strength ( ≥ 20 N/mm2) allows the material to be used not only in residential premises, but also in garages, warehouses, etc. (with low intensity of mechanical influences)
• arrangement of “warm floor” systems using water heating elements.
| Proportions of water for mixing, l per 25 kg | 3.5-4.0 |
| Mortar mixture maturation time, min | 3-5 |
| Suitability time of the prepared solution for use, min., not less than | 60 |
| Recommended layer thickness min/max, mm | 10/40 |
| Recommended layer thickness with the addition of fractionated crushed stone (2-5 mm), mm, max | 100 |
| The time of readiness of the screed after laying, not less than, days: - technological movement - laying tiles - painting, gluing coatings with organic-based adhesives |
1 7 28 |
| Substrate and ambient temperature during operation, from ... to, °C | +5 ... +30 |
POLIMIN PC-5 FIBRE REINFORCED SCREED cement screed for arranging and leveling floors, before laying tiles and other coatings, inside and outside buildings.
Technological properties of the PC-5 screed allow leveling the surface of existing concrete and cement-sand screeds with a graded strength of at least 20 MPa before laying facing tiles, other floor layers: self-leveling floors, etc. The screed allows for the arrangement of water-heated floor systems in strict compliance with the recommendations of the manufacturer of these systems, the thickness of the mortar layer above the heating element must be at least 25 mm.
Thanks to the improved formula, the product provides:
• easy distribution and leveling of the screed at an angle (performance of the screed)
• wide range of layer thicknesses (10–100* mm) ensures its use in various structures
• compressive strength ( ≥ 20 N/mm2) allows the material to be used not only in residential premises, but also in garages, warehouses, etc. (with low intensity of mechanical influences)
• arrangement of “warm floor” systems using water heating elements.
| Proportions of water for mixing, l per 25 kg | 3.5-4.0 |
| Mortar mixture maturation time, min | 3-5 |
| Suitability time of the prepared solution for use, min., not less than | 60 |
| Recommended layer thickness min/max, mm | 10/40 |
| Recommended layer thickness with the addition of fractionated crushed stone (2-5 mm), mm, max | 100 |
| The time of readiness of the screed after laying, not less than, days: - technological movement - laying tiles - painting, gluing coatings with organic-based adhesives |
1 7 28 |
| Substrate and ambient temperature during operation, from ... to, °C | +5 ... +30 |