Cement screed for arranging and leveling the floor before laying tiles and other coatings inside and outside buildings.
Thanks to the improved special formula, the product provides:
• the ability to easily distribute and level the screed at an angle (perform a screed);
• a wide range of layer thicknesses (10-80** mm.) ensures use in mortise structures;
• compressive strength (≥ 20 MPa) allows the product to be used not only in residential areas, but also in garages, warehouses, etc. (with weak mechanical impact);
• installation of “warm floor” systems.
| Water consumption of the mixture per 25 kg bag, l | 3.5-4.25 |
| Maturation time of the mortar mixture, min. | 3-5 |
| Potency of the prepared solution to use, not less than, min | 20 |
| Recommended layer thickness, min/max 10 / 40 | 10 / 40 |
| Recommended layer thickness with the addition of fractionated crushed stone (2-5 mm), max, mm | 80 |
| Estimated coverage area from a bag of 25 kg of dry mix, with a layer thickness of 10 mm, m² | 1.3 |
| Ready-to-use time of the screed after laying days, not less than: - technological movement - laying tiles - painting, gluing coatings with organic-based adhesives |
1 3 7 |
| Compressive strength, N/mm² ≥ | 20 |
| Tensile strength when bending, N/mm² ≥ | 4 |
| Base and ambient temperature during operation, °C, from...to | +5...+30 |
| Operating temperature, °C, from...to | -30...+70 |
Cement screed for arranging and leveling the floor before laying tiles and other coatings inside and outside buildings.
Thanks to the improved special formula, the product provides:
• the ability to easily distribute and level the screed at an angle (perform a screed);
• a wide range of layer thicknesses (10-80** mm.) ensures use in mortise structures;
• compressive strength (≥ 20 MPa) allows the product to be used not only in residential areas, but also in garages, warehouses, etc. (with weak mechanical impact);
• installation of “warm floor” systems.
| Water consumption of the mixture per 25 kg bag, l | 3.5-4.25 |
| Maturation time of the mortar mixture, min. | 3-5 |
| Potency of the prepared solution to use, not less than, min | 20 |
| Recommended layer thickness, min/max 10 / 40 | 10 / 40 |
| Recommended layer thickness with the addition of fractionated crushed stone (2-5 mm), max, mm | 80 |
| Estimated coverage area from a bag of 25 kg of dry mix, with a layer thickness of 10 mm, m² | 1.3 |
| Ready-to-use time of the screed after laying days, not less than: - technological movement - laying tiles - painting, gluing coatings with organic-based adhesives |
1 3 7 |
| Compressive strength, N/mm² ≥ | 20 |
| Tensile strength when bending, N/mm² ≥ | 4 |
| Base and ambient temperature during operation, °C, from...to | +5...+30 |
| Operating temperature, °C, from...to | -30...+70 |