The adhesive mixture is intended for gluing insulation boards (expanded polystyrene, graphite expanded polystyrene and mineral wool) when installing thermal insulation systems outside buildings and for creating a waterproofing reinforcing layer on the boards of the above insulation materials. Recommended for multi-storey and cottage construction.
| Water demand per 25 kg of dry mix: - l / 1 kg - l / 25 kg |
0.20 - 0.22 5.0 - 6.0 |
| Dry mix consumption, kg/m²: for glueing insulation for arranging the reinforcing layer |
5,0-5,5 5,0-6,0 |
| Suitability of the mortar mix, no less than, h | 2 |
| Open time, no less than, minutes | 20 |
| The temperature of the base and ambient temperature during application, °С | +5 ... +30 |
| Operating temperature, ºС | -30 … +70 |
| Frost resistance, not less than, cycle | 50 |
| Shelf life, months | 12 |
The adhesive mixture is intended for gluing insulation boards (expanded polystyrene, graphite expanded polystyrene and mineral wool) when installing thermal insulation systems outside buildings and for creating a waterproofing reinforcing layer on the boards of the above insulation materials. Recommended for multi-storey and cottage construction.
| Water demand per 25 kg of dry mix: - l / 1 kg - l / 25 kg |
0.20 - 0.22 5.0 - 6.0 |
| Dry mix consumption, kg/m²: for glueing insulation for arranging the reinforcing layer |
5,0-5,5 5,0-6,0 |
| Suitability of the mortar mix, no less than, h | 2 |
| Open time, no less than, minutes | 20 |
| The temperature of the base and ambient temperature during application, °С | +5 ... +30 |
| Operating temperature, ºС | -30 … +70 |
| Frost resistance, not less than, cycle | 50 |
| Shelf life, months | 12 |